Gold refining


Before starting gold refining business you choose right tools, supplies and chemicals. The demand for scrap jewelry is rising and very popular in front of gold producers. The dental and electronics industry frequently used refined gold products. So basically you sold the gold.
Difficulties

1) Make sure you need the financial support to start a gold refining business.
2) Search gold refine business. work free until and improve your skills. Give interview the owner by phone or Personally meet him and ask him how he started his gold refining business.
3) Once you have developed the skills needed to start your gold refining business. Then decide which type of gold refining business you want to start.
4) Your business plan should explain how you will get customers (jewelry repair departments., jewelry manufacturers etc.). Include how you plan to operate each day. Set up a financial plan to monitor your cash flows. Go to your local city or county office and apply for a permit or license to operate your business. Apply for your state tax ID number too.
These steps will help you get start your gold refining business. 
*************
Extract gold from scraps electronic items
1) Collect any gold-containing metal scraps to which you have access, including jewelry, computer processors, old telephone wiring or gold tooth crowns. Keep in mind that outdated electronics items are produce enough gold.


2) For scrap metal choose correct size of container, jar and chemicals. In which you wish to refined. You need container capacity 300 milliliters, 30 milliliters nitric acid, and 120 milliliters of hydrochloric acid for every ounce of scrap gold metal.



3) Apply all safety gear correctly before working with any chemicals. The acids involved in this process are highly corrosive and react strongly.







4) Add your scrap materials and the appropriate amount of nitric acid, as mentioned above, to the smaller of your plastic containers. Wait 30 minutes before adding the hydrochloric acid. Let the chemical reaction develop overnight to be sure that all of the gold has dissolved.
5) Filter the particles out of the acid in the plastic container by attaching a Buckner funnel filter and pouring the remaining liquid into the larger of the plastic containers. The resulting acid will be deep green and translucent.

6) Create a urea and water solution boiling a quart of water and combining it with one pound of urea Pour this mixture into the acid slowly. until no chemical reaction can be observed. This process raises the pH levels of the acid, there is eliminating the nitric acid.

7) Heat a quart of water. and add the sodium bisulfite to the boiling water in the ratio of one ounce of sodium bisulfite for every ounce of metal being refined. Pour this mixture slowly into the acid and wait for a reaction.

8) Observe the muddy separation. that collects at the bottom of the acid container. This substance is pure gold. Extract the gold from the container. using a filter.
Substance three time filter with clean water. and The result will nearly 100 percent gold.

Tips & Warnings
1) Some experts recommend using SubZero in place of nitric acid. This nitric acid replacement reacts in lower quantities and does not create as many fumes.
2) Do not attempt this process if you do not have adequate chemistry lab experience.
*************